Symposium on stress-corrosion cracking of metals

held at Philadelphia, Pa., November 29-30 and December 1, 1944

Symposium on stress-corrosion cracking of met ...
American Society for Testing a ...
Not in Library

My Reading Lists:

Create a new list

Check-In

×Close
Add an optional check-in date. Check-in dates are used to track yearly reading goals.
Today


Buy this book

Last edited by WorkBot
December 21, 2011 | History

Symposium on stress-corrosion cracking of metals

held at Philadelphia, Pa., November 29-30 and December 1, 1944

This edition doesn't have a description yet. Can you add one?

Publish Date
Language
English
Pages
495

Buy this book

Edition Availability
Cover of: Symposium on stress-corrosion cracking of metals
Cover of: Symposium on stress-corrosion cracking of metals
Symposium on stress-corrosion cracking of metals: held at Philadelphia, Pa., November 29-30 and December 1, 1944
1945, Pub. jointly by American society for testing materials and Institute of metals division, American institute of Mining and metallurgical engineers, New York
in English
Cover of: Symposium on stress-corrosion cracking of metals
Cover of: Symposium on stress-corrosion cracking of metals
Symposium on stress-corrosion cracking of metals
1945, Pub. jointly by American Society for Testing Materials and Institute of Metals Division, American Institute of Mining and Metallurgical Engineers, New York, N.Y.
in English

Add another edition?

Book Details


Edition Notes

Published jointly by American Society for Testing Materials and Institute of Metal Division, American Institute of Mining and Metallurgical Engineers.

Bibliogr.

16

Published in
Philadelphia, PA

Classifications

Library of Congress
TA'462'A48

The Physical Object

Pagination
viii, 495 p. :
Number of pages
495

ID Numbers

Open Library
OL21658106M

Community Reviews (0)

Feedback?
No community reviews have been submitted for this work.

Lists

This work does not appear on any lists.

History

Download catalog record: RDF / JSON / OPDS | Wikipedia citation
December 21, 2011 Edited by WorkBot merge works
February 9, 2011 Edited by AMillarBot merge authors
December 15, 2009 Edited by WorkBot link works
November 3, 2008 Created by ImportBot Imported from The Laurentian Library MARC record